品牌
其他厂商性质
所在地
性能项目 | 测试方法 | 单位 | 指标(典型数据) | |||||
厚度 | | µm | 18 | 20 | 30 | 40 | 60 | |
厚度偏差 | ASTM-252-78 | % | ±3.0 | ±3.0 | ±2.5 | ±2.0 | ±1.5 | |
拉伸强度 | MD | ASTM D-882 | MPa | 150 | 150 | 160 | 145 | 140 |
TD | ASTM D-882 | MPa | 300 | 300 | 300 | 280 | 280 | |
断裂伸长率 | MD | ASTM D-882 | % | 170 | 170 | 170 | 175 | 180 |
TD | ASTM D-882 | % | 50 | 50 | 55 | 55 | 60 | |
摩擦系数 | T/T-US | ASTM D-1894 | | 0.35 | 0.35 | 0.35 | 0.35 | 0.35 |
T/O-US | ASTM D-1894 | | 0.40 | 0.40 | 0.40 | 0.40 | 0.40 | |
热收缩率 | MD | ASTM D-1204 | % | 4.0 | 4.0 | 4.0 | 4.0 | 4.0 |
TD | ASTM D-1204 | % | 2.0 | 2.0 | 2.0 | 2.0 | 2.0 | |
雾度 | ASTM D-1003 | % | 1.0 | 1.0 | 1.1 | 1.2 | 1.5 | |
光泽度 | ASTM D-2457 | | 90 | 90 | 90 | 90 | 90 | |
润湿张力 | ASTM D-2578 | Dyn | 38 | 38 | 38 | 38 | 38 |